Chemistry:
Nickel 63.0 Sulfur 0.01 max
Copper 27.0-33.0 Silicon 0.5 max
Carbon 0.25 max Aluminum 2.30-3.15
Manganese 1.5 max Titanium 0.35-0.85
Iron 2.0 max
By adding Aluminum and Titanium to this nickel/copper alloy, followed by an age hardening process, this enhances the physical properties, giving the material greater strength and hardness.
Marine Applications for K-500:
TW Metals stocks a diverse range of diameters in K-500. If you want to learn more about our product offerings or a get a quote on K-500, please contact us or give us a call!
Advantages & Specifications of K500:
Stocked to the QQN 286 Form 2 Rev F & G spec for marine applications. Available for the Oil & Gas Industries to the QQN 286 Form 1 Rev E spec + NAVE MRO175